Mar 11, 2024 ご伝言

Non-Oriented Electrical Steel Manufacturer

Non-oriented electrical steel

The magnetic properties of non-oriented electrical steels strongly depend on the silicon content, the cleanliness of the steel, the thickness of the steel sheet, and the grain size and texture of the final lamination.

Non-oriented electrical steel, often referred to as non-grain-oriented electrical steel or simply non-oriented steel, is a type of soft magnetic material used in the construction of electrical machines and devices. It is an essential component in the manufacturing of motors, generators, transformers, and other electromagnetic devices that require efficient and low-loss magnetic properties.

利用可能 厚さ 内径 直径
0.15,0.20 950-1000 508±10
0.30 0.35 0.50 0.70 0.75 0.80 0.85 1000-1250 508±10

Camber within 2m
ミリメートル %
0.15 ±0.012 Less than or equal to 0.010 0~+1.5 Less than or equal to 1.5 Less than or equal to 1.0
0.2 ±0.012 Less than or equal to 0.010
0.3 ±0.015 Less than or equal to 0.012
0.35 ±0.015 Less than or equal to 0.012
0.5 ±0.020 Less than or equal to 0.015
0.7 ±0.030 Less than or equal to 0.025
0.75 ±0.030 Less than or equal to 0.025
0.8 ±0.040 Less than or equal to 0.030
0.85 ±0.040 Less than or equal to 0.030

Note: a. Traverse thickness deviation refers to the thickness difference between the sheet center and 15mm from the edge.

 