904L Stainless Steel Buttweld Fittings
中国の大手サプライヤーおよびメーカーとして、GNEE Steel はコスト効率の高い-ニッケル- ベースの合金製品を提供しています。
- 電子メールを送信-:ss@gneesteel.com
- 電話番号:+8615824687445
ASTM B366 WP 904L Stainless Steel Pipe Reducer
Our SS 904L Buttweld fittings are acclaimed in the market owing to its dimensional accuracy. SS 904L Buttweld Fittings are used in various industries such as sugar mills, pumps & petrochemicals cement & construction industries. Alloy 904L Buttweld Fittings are available in different grades and sizes, shapes. We are providing these stainless steel pipe fittings in assorted dimensions & sizes details specified by clientele.
904L Stainless Steel Buttweld Concentric Reducer Fittings Chemical Composition
| 0.02 | |
| シリコン (Si) | 0.70 |
| 2.00 | |
| 0.03 | |
| 0.01 | |
| 19.00 - 21.00 | |
| 24.00 - 26.00 | |
| 0.15 | |
| 4.00 - 5.00 | |
| 1.20 - 2.00 | |
| 鉄 (Fe) |
| C | H | P | L | L | ||||
| 8.0 | 13.5 | 75 | 160 | 2502) | 60 | |||
| Rp0.22 | 2403) | 2203) | 2203) | 2304) | 2305) | 2306) | ||
| Rp1.02 | 2703) | 2603) | 2603) | 2603) | 2603) | 2503) | ||
| Rm2 | 530 - 7303) | 530 - 7303) | 520 - 7203) | 530 - 7304) | 530 - 7305) | 520 - 7206) | ||
| J | - | 100 | 100 | 100 | - | 120 | ||
| J | - | 60 | 60 | - | 60 | 90 | ||
Industries & Applications Where Our 904L Stainless Steel Buttweld Fittings Are Used in those areas:

A:30% T/T in advance, 70% balance before shipment or based on copy of bill of lading or L/C at sight.
Q: Can I send samples?
人気ラベル: 904l stainless steel buttweld fittings, China 904l stainless steel buttweld fittings suppliers, 310 バットウェルドフランジ
あなたはおそらくそれも好きでしょう
お問い合わせを送る